A335wimbo wa chuma usio na bahari
ASTM A335 Mawizi ya wizi yanaweza kuchukuliwa kwa kumaliza joto au mchoro wa baridi,Na kutekeleza matibabu ya joto ifuatayo。Tafsiri hii inahusu“Kromium Molybdenum”wimbo usio na bahari,Kuna upinzani mzuri wa upinzani na nguvu kubwa ya joto。kwa ujumla,ASTM A335 P11、P22 na P91 Mafuriko yanatumiwa kwa ajili ya kizazi cha umeme na mafuta na gesi chini ya mto,P5 na P9 Grade kwa matumizi maboresho。
maelezo ya bidhaa
ASTM A335 Mawizi ya wizi yanaweza kuchukuliwa kwa kumaliza joto au mchoro wa baridi,Na kutekeleza matibabu ya joto ifuatayo。Tafsiri hii inahusu“Kromium Molybdenum”wimbo usio na bahari,Kuna upinzani mzuri wa upinzani na nguvu kubwa ya joto。kwa ujumla,ASTM A335 P11、P22 na P91 Mafuriko yanatumiwa kwa ajili ya kizazi cha umeme na mafuta na gesi chini ya mto,P5 na P9 Grade kwa matumizi maboresho。
Parameters
jina la bidhaa | A335wimbo wa chuma usio na bahari | |
default | EN/DIN/JIS/ASTM/BS/ASME/AISIdarasa | |
nje ya diameter | bila ufukweni:1/4"-36" | ikifunga:21.3mm-3620mm |
Kizungumzo:1/2"-10" | Mfuko wa viwanja/Kipimo cha kisasa:15x15-400x600mm | |
uchi wa ukuta | bila ufukweni:1.25mm-50mm | ikifunga:1.65mm-65mm |
duru | 3-12mchezo,Support customizion | |
surfekazi | mwanga、polishing、color | |
Huduma nyingine | wanaohamasisha(CNC)、grinding(CG)、matibabu ya joto、anaonyesha、kuchagua acid、polishing、ikizunguka、forge、kifupi、bend、Utafiti mdogo wa scale, etc | |
uzalishaji wa kemikali
A335 | UNS | C≤ | Mn | P≤ | S≤ | Si≤ | Cr | Mo |
P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | – | 0.44~0.65 |
P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | – | 0.44~0.65 |
P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
Tatizo za Kichaniki
A335 | UNS | hutoa nguvuksi | nguvu ya kifuaksi | paper size % |
P1 | K11522 | 30 | 55 | 30 |
P2 | K11547 | 30 | 55 | 30 |
P5 | K41545 | 40 | 70 | 30 |
P9 | S50400 | 30 | 60 | 30 |
P11 | K11597 | 30 | 60 | 20 |
P12 | K11562 | 32 | 60 | 30 |
P22 | K21590 | 30 | 60 | 30 |
P91 | K91560 | 60 | 85 | 20 |
Kifaa cha programu
Tafsiri hii inahusu“Kromium Molybdenum”wimbo usio na bahari,Kuna upinzani mzuri wa upinzani na nguvu kubwa ya joto。kwa ujumla,ASTM A335 P11、P22 na P91 Mafuriko yanatumiwa kwa ajili ya kizazi cha umeme na mafuta na gesi chini ya mto,P5 na P9 Grade kwa matumizi maboresho。